How does HYSF prevent Cathodic Delamination?

Cathodic Delamination is a common failure where the rubber peels off the metal shell due to hydrogen gas evolution in systems using Sacrificial Anodes. HYSF prevents this by using specialized Primers and a rigorous Sandblasting process during manufacturing to create an unbreakable chemical bond between the metal and the elastomer.

If your ROV has Zinc anodes, the whole frame is electrically “active.”

  • The Problem: The cathodic protection system generates hydrogen ions at the metal surface. If the rubber bond is weak, this gas pressure will “blow” the rubber off the metal, causing leakage.
  • Our Solution: We use a two-step primer system and sandblast the metal to SA 2.5 standard to increase surface area.
  • Result: Our bond strength exceeds the tear strength of the rubber itself (i.e., the rubber will tear before it peels off the metal).
Billede af John Zhang

John Zhang

(CEO og ledende ingeniør)
E-mail: info@hysfsubsea.com
Med over 15 års ekspertise inden for undervandsforbindelsesteknologi leder jeg HYSF's R&D-team med at designe højtryksløsninger (60MPa). Mit fokus er at sikre pålidelighed uden lækage for ROV'er, AUV'er og offshore-instrumentering. Jeg fører personligt tilsyn med valideringen af vores prototyper af brugerdefinerede forbindelser.

Har du et komplekst teknisk spørgsmål?

Gennemprøvede løsninger i marken

Et udstillingsvindue for vores vellykkede samarbejde med globale partnere inden for maritim robotteknologi, energi og forskning. Hvert projekt afspejler vores engagement i nul-lækage-integritet og driftssikkerhed.

Start dit undervandsprojekt med HYSF

Uanset om du har brug for et hurtigt tilbud på standardstik eller en kompleks, tilpasset kabelsamling, er vores ingeniørteam klar til at hjælpe. Forvent et teknisk svar inden for 12 timer.

John Zhang

ADMINISTRERENDE DIREKTØR

Jason Liu
Kevin Wang
Cindy Chen
Lily Li
Demo af kontaktformular