Light tarnish (darkening) on gold pins is often just surface oxidation or dirt and can be cleaned with DeoxIT® or a mild contact cleaner. If you see green copper oxide or pitting (holes in the plating), the gold layer has been compromised. In this case, the connector must be replaced to avoid reliability issues.

Gold korrodiert nicht, aber das darunter liegende Metall könnte korrodieren.

  • Do Not Sand: Never use sandpaper or steel wool on gold-plated pins! You will strip the plating off entirely.
  • Mild Abrasive: For stubborn tarnish, you can use a very fine Scotch-Brite pad or a pencil eraser very gently, then clean with alcohol.
  • Prevention: Green corrosion usually means the connector was unmated while wet. Always rinse and dry before storage.
Bild von John Zhang

John Zhang

(CEO & leitender Ingenieur)
E-Mail: info@hysfsubsea.com
Mit über 15 Jahren Erfahrung in der Unterwasserverbindungstechnik leite ich das Forschungs- und Entwicklungsteam von HYSF bei der Entwicklung von Hochdrucklösungen (60MPa). Mein Schwerpunkt liegt auf der Gewährleistung einer leckagefreien Zuverlässigkeit für ROVs, AUVs und Offshore-Instrumente. Ich beaufsichtige persönlich die Validierung unserer kundenspezifischen Steckverbinder-Prototypen.

Sie haben eine komplexe technische Frage?

Bewährte Lösungen in der Praxis

Ein Schaufenster unserer erfolgreichen Zusammenarbeit mit globalen Partnern aus den Bereichen Schiffsrobotik, Energie und Forschung. Jedes Projekt spiegelt unser Engagement für leckfreie Integrität und Betriebssicherheit wider.

Starten Sie Ihr Unterwasserprojekt mit HYSF

Ganz gleich, ob Sie ein schnelles Angebot für Standardsteckverbinder oder eine komplexe kundenspezifische Kabelkonfektion benötigen, unser Technikteam steht für Sie bereit. Erwarten Sie eine technische Antwort innerhalb von 12 Stunden.

John Zhang

CEO

Jason Liu
Kevin Wang
Cindy Chen
Lily Li
Kontakt-Formular Demo