標準的なステンレス鋼(316Lであっても)は、機械加工後もわずかな磁性を保持することがあります。.
- Material Selection: We carefully select raw materials with low magnetic permeability (µ).
- プロセス We avoid using nickel underplates (which are magnetic) in the plating process for these specific orders.
- Verification: We can provide a Magnetic Permeability Test Report with the shipment to certify the component is “Non-Magnetic.”