How does HYSF prevent Cathodic Delamination?

Cathodic Delamination is a common failure where the rubber peels off the metal shell due to hydrogen gas evolution in systems using Sacrificial Anodes. HYSF prevents this by using specialized Primers and a rigorous Sandblasting process during manufacturing to create an unbreakable chemical bond between the metal and the elastomer.

If your ROV has Zinc anodes, the whole frame is electrically “active.”

  • The Problem: The cathodic protection system generates hydrogen ions at the metal surface. If the rubber bond is weak, this gas pressure will “blow” the rubber off the metal, causing leakage.
  • Our Solution: We use a two-step primer system and sandblast the metal to SA 2.5 standard to increase surface area.
  • Resultat: Our bond strength exceeds the tear strength of the rubber itself (i.e., the rubber will tear before it peels off the metal).
Bilde av John Zhang

John Zhang

(administrerende direktør og ledende ingeniør)
E-post: info@hysfsubsea.com
Jeg har over 15 års erfaring med undervannskoblingsteknologi og leder HYSFs FoU-team som utformer høytrykksløsninger (60 MPa). Jeg fokuserer på å sikre pålitelighet uten lekkasje for ROV-er, AUV-er og offshore-instrumentering. Jeg fører personlig tilsyn med valideringen av våre tilpassede prototyper.

Har du et komplisert teknisk spørsmål?

Utprøvde løsninger i felten

Et utstillingsvindu for vårt vellykkede samarbeid med globale partnere innen marin robotikk, energi og forskning. Hvert prosjekt gjenspeiler vår forpliktelse til null lekkasjeintegritet og driftssikkerhet.

Start ditt subseaprosjekt med HYSF

Enten du trenger et raskt tilbud på standardkontakter eller en kompleks, spesialtilpasset kabelmontering, står ingeniørteamet vårt klart til å hjelpe deg. Du kan forvente et teknisk svar innen 12 timer.

John Zhang

ADMINISTRERENDE DIREKTØR

Jason Liu
Kevin Wang
Cindy Chen
Lily Li
Demo av kontaktskjema